Visit http://www.esabna.com/ for more information about our products.
Florence, SC – ESAB introduces the PUROX Metal Master GT II hand-held oxyfuel cutting outfit. This top-of-the-line outfit contains rugged components built for medium- and heavy-duty performance in a wide range of industrial, construction, maintenance and other metalworking applications. The heavy-duty toolbox houses a superior combination of components, featuring three PUROX® cutting tips and one heating head.
The kit offers a cutting range up to four inches (100 mm) and a heating range up to 30 cfh acetylene (44,000 Btu/hr). With optional heads and nozzles, these ranges can be extended to up to eight inches (203 mm) and up to 200 cft (294,000 Btu/hr). The kit features ESAB’s R-72 regulators with solid brass bodies and built-in regulator burnout (RBO) protection. ESAB regulators incorporate a patented internal baffle design to prevent injury from cylinder-based fires. The regulators also feature color-coded gauges for easy gas identification. Brass body construction ensures long service life. These regulators are built for years of trouble-free performance with minimum maintenance. The Metal Master GT II kit comes with a lifetime warranty on the torches and regulators.
With more than 100 years of experience, ESAB Welding & Cutting Products is one of the world’s largest and most skilled manufacturers of welding and cutting equipment and welding filler metals. Ensuring customer satisfaction, a wide range of ESAB products carry the 100% Satisfaction Guarantee. Recognized as the technological leader in the industry, ESAB is committed to providing customized solutions for their customers. For more information on the company, visit www.esabna.com or call 1-800-ESAB123.